Volkswagen Golf Mk7 Service & Repair Manual: Corrosion protection measures for wing surface in contact with wheel housing liner

Note: new replacement Volkswagen Golf Mk7 wings without factory sealant need corrosion protection applied to the groove area — this page explains why, to prevent the wheel housing liner from trapping moisture against bare metal.

  Note
  The corrosion protection measure is to be carried out in the groove of the wing of all new replacement parts which have not had the additional sealant applied at the factory.
  The additional sealant is intended to prevent the wheel housing liner from possibly “scouring” the groove of the wing, which could cause corrosion.
–  Apply surfacer on inside and outside of wing.
–  After surfacer has been applied and has dried, apply and spread sealant -D 511 500 A2- in the contact area of wheel housing liner (groove of wing).

Corrosion protection measures for wing surface in contact with wheel housing liner

MaЯ a -  20 mm
   Height of seal
MaЯ b -  10 mm
   Width of seal
  Note
-Dimension b- can vary because the width of the edge of the groove differs among wings. Always ensure that the entire edge of the groove is sealed.
 
Before installing, seal inside of wheel arch and web plate with cavity sealant.
Product information:
  → Chapter „Anti-corrosion materials“

    Questions & answers

    Corrosion protection measures for wing surface in contact with wheel housing liner — Volkswagen Golf Mk7

    Do new Golf Mk7 replacement wings need corrosion protection in the liner groove?
    Yes. All new wings that have not been factory-treated must have the groove area coated before fitting the wheel housing liner.
    Pre-treatment of bonded surfaces when renewing laser-welded roofs
    Using P180-grade sandpaper, dry-sand cathodic dip primer on bonding surface for roof → Item down to bare metal.   ...

    Notes on treating corroded fold areas
    Examples for corrosion in the fold area of bonnet, door or rear lid –  Remove corrosion using → Chapter „Pneumatic br ...